AXAR PP - D
Weight
g/m²
|
Tensile Strength
N/5cm
|
Elongation
%
|
| |
MD
|
CD
|
MD
|
CD
|
| 14 |
22 |
21 |
50-60 |
60-70 |
| 15 |
24 |
23 |
50-60 |
60-70 |
| 17 |
26 |
25 |
50-60 |
60-80 |
| 20 |
36 |
32 |
60-80 |
70-80 |
| 25 |
46 |
42 |
60-80 |
70-90 |
| 30 |
56 |
54 |
60-80 |
70-90 |
| 35 |
66 |
66 |
60-80 |
70-90 |
| 40 |
70 |
70 |
70-90 |
70-90 |
| 50 |
90 |
90 |
70-90 |
70-90 |
| 60 |
102 |
102 |
70-90 |
70-90 |
| 70 |
115 |
115 |
70-90 |
70-90 |
| 85 |
125 |
120 |
70-90 |
70-90 |
| 95 |
140 |
130 |
70-90 |
70-90 |
Test Method: UNI EN 29073 p.3
|